Blow Molding "WS2 increased product quality, reduced streaking and drag. Machine settings maintained on constant basis." — Mr. Frank Rukavina, K&M Plastics, Elk Grove Village, Illinois
Injection Molding "WS2 provided exceptional release while eliminating unscrewing problems with chucks. There was a decrease in energy consumption on motors from 21 amps to 15 amps." — Mr. Michael Vavrik, Ethyl Corporation, Alsip, Illinois
"Tooling coated with WS2 filled faster at less temperature and pressure. Cycle time reduced between 6% to 8% and rejects reduced to less than a half a percent." — Mr. Richard Kanowske, Tandy Bell & Howell, Northbrook, Illinois
"We reduced our temperature and pressure with WS2 on the average of 8% to 11%. Stress was reduced on larger parts." — Mr. Charles Cizek, Armin Tool & Manufacturing, South Elgin, Illinois
"We experienced a decrease in pressure between 200 and 300 lbs. and a drop in temperature of 10%." — Mr. Michael Fraas, Hoffer Plastics, South Elgin, Illinois
"WS2 coating eliminated our flow problems on thin walled parts and helped to increase our production substantially." — Mr. Miram Wooley, Samsonite luggage, Denver Colorado
"The WS2 coating improved our cycle time, reduced stress in the parts and provided excellent release condition." — Mr. Larry Jones, Jones Plastics, Louisville, Kentucky
|